I have one of the NOE Brass 432-265 RF molds RG4 PB-GC molds, do these molds need to be smoked lightly before use? I thought only alum molds need to ne smoked.
My thinking is any mould that has not been “seasoned” can use it. It gives it time to start oxidizing and forming a patina. It will also help a brass mould keep from “tinning”
If a mould is cleaned and heated good and still getting wrinkled bullets give it a try.
Al gives some excellent advice, so I will just add my two cents, FWIW. The majority of NOE molds that I have are Brass, I have a few alum also. The biggest thing I’ve learned about brass is clean, clean, clean the mold when You first receive it. I use HOT, nearly boiling water, dish soap(dawn) and a toothbrush. Heat cycle per the instructions sent with the mold, and lastly brass molds seem to work better with a couple or three pouring sessions. I think it has to do with the brass getting a patina to it, and the quicker it develops a patina, the less likely it will “tin” like Al mentions… OH, and touch the pins with a Q-tip Dampened(not dripping) with sprue plate lube every 30 or so pours when pin are HOT, it helps out.
Thank you Gentlemen for the great Information. Bones37 you suggested I lube the pins every 30 casts, which area should I lube on the pins? Do you know what the as cast diameter these bullets come out? Was think of trying alox and pan lubing the bullets when I get to casting some later this month. Need to make a pan lube cake cutter.
Thank you Gentlemen for the great Information. Bones37 you suggested I lube the pins every 30 casts, which area should I lube on the pins? Do you know what the as cast diameter these bullets come out? Was think of trying alox and pan lubing the bullets when I get to casting some later this month. Need to make a pan lube cake cutter.
Thanks Again, MickeyJr.
I touch a very lightly dampened Q-tip on the tips of the pins( the part of the pin that makes the hollow point cavity.) Just don’t over-do it. If too much sprue plate lube is used, it will migrate back into the cavities causing wrinkling and poor fill out. It seems to help the pins “season” and the bullets will jump right off.
One thing which i noticed…I use pure lead and 2 % sn thats usually best alloy for airguns. It gives like 7-9 BHN. Couple weeks ago i casted some .257 bullets for my friend and use alloy which gave me 18 BHN.He needed harder bullets for his “real” rifle. Bullets drops out for mold so easy only thing to do is open a mold 😮 And i didin´t even smoked that mold and bullet were flawless. I quess alloy also has something to do it…