      What is the bet solution/technique to fix the swarf left on the mold.

    Viewing 8 replies - 1 through 8 (of 8 total)
    • Author
      Replies
    • #511088
      Hugh Kuhns
      Participant
        Up
        0
        Down
        ::

        I’m not sure from the photo if that is a machining problem. That looks like lead deposits around the sprue plate holes. And I noticed that the sprue plate has been reversed and has drag marks from use…in both positions. Are you using proper lubrication? I would suggest that the mould be taken apart and cleaned and done in the way suggested by NOE…hot water, toothbrush and dish soap.  Carefully clean the lead deposits from the sprue plate and mould surfaces with a wooden popsicle stick, or wooden kitchen match…never use a metal instrument. Once clean lube with NOE lube that came with it when new. Check the sprue plate tightness. It should be able to move back and forth on it’s own weight and swing freely. If it is not as I described, but a mould imperfection, you should contact Al at NOE for his expert opinion and solution.

        762sultan

        #511089
        rsterne
        Participant
          Up
          0
          Down
          ::

          I had the same thing, on one side only…. I cleaned it up very carefully using a 1/8″ diameter round fine grit diamond file…. Use a magnifying loupe so that you can really see what you are doing, and don’t round or bevel the corner, just take off the flashing….

          Bob

          #511090
          Hugh Kuhns
          Participant
            Up
            0
            Down
            ::

            I discovered after posting a reply that this is an air gun mould . I believe that different rules apply to them as they are smaller and more difficult to cast with. I would follow rstern’s advice as he is an experienced air gun shooter.

            762sultan

            #511091
            tnt76
              Up
              0
              Down
              ::

              It’s not lead deposits, it is flashing, as it was there before use.  I have prepped the mold according to NOE guidelines before use also.  The darker marks are from the sprue plate, which I think is from smoking the cavities and dragging the soot.  And the sprue plate has been reversed so that my temp probe lead can be taped to the handles, however I did do a preliminary casting beforehand.
              As Bob has also experienced, it is machining flashing.
              I will wait for Al’s recommendation also, or just do as Bob did.

              250-34 pellet mold by the way.

              #511092
              SwedeNelson
              Keymaster
                Up
                0
                Down
                ::

                tnt76
                A good cleaning with a tooth brush will get about 80% of the burrs off.
                The balance you can get with your thumb nail or a round tooth pick.
                The real bad places I use a copper penny.
                I don’t like to use a file or even a diamond file – it takes to much off to fast.
                Slow and easy is what I look for.
                We try to get them cleaned up before we ship them, but some get through – Sorry

                You can send it back and will fix it.

                Bullet maker, maker
                Al Nelson 

                #511093
                tnt76
                  Up
                  0
                  Down
                  ::

                  Ok, thanks, I will give that a go.
                  I’m in Australia, so shipping back for a little tidy up obviously isn’t worth it.

                  Thanks again.

                  #511094
                  michaellovett
                    Up
                    0
                    Down
                    ::

                    As suggested, use a round toothpick, put it into the cavity, and press against the flashing and pull out. The flashing is very thin, and comes off easily. ;)

                    KnifeMaker

                    #511095
                    tnt76
                      Up
                      0
                      Down
                      ::

                      So I have done as suggested, and worked over the mold to rid it of the machining dags, starting with the side of a plastic paint scraper and broke the chips off with a back and forward technique, then wrapping a 1/16 drill bit with 400grit wet and dry sandpaper and spinning by hand, while maintaining the curved profile of the head of the pellet. Then polishing with some scotchbrite style fine cloth by hand. It now looks almost flawless.
                      And while also adding a 1.5 degree leade to the marauder (to suit the 50gr BBT’s), and casting a new batch of these 34.4gr in pure lead, my 50 meter groups have shrunk from 4-6″ to around 1″, much happier now.  Bases are not perfect either, so I might play a bit more with casting temp, currently at 750f and mold temp floating around 400f – 415f, also the pins heated with butane torch.

                      Looking promising.

                    Viewing 8 replies - 1 through 8 (of 8 total)